Veröffentlichungen

Prediction and measurement of microsegregation and microstructural evolution of directionally solidified superalloys

B. Böttger, U. Grafe, D. Ma and A. Schnell

Journal:

Volume:

Issue:

Pages:

Conference Name:

Superalloys 2000 : proceedings of the Ninth International Symposium on Superalloys ... held September 17 - 21, 2000, Seven Springs, PA / sponsored by the TMS Seven Springs International Symposium Committee, in cooperation with the TMS High Temperature Alloys Committee ... Ed. by T. M. Pollock ... Minerals, Metals and Materials Society / High Temperature Alloys Committee